Alloy Digest (1985) 34 (1): Ni-309.
Published: 01 January 1985
... Nickel Alloy 600 is a nickel-base alloy intended for use in a wide range of applications from cryogenic to temperatures above 2000 F, where high-temperature properties and resistance to oxidation or corrosion are desired. This alloy has been used in nuclear, petroleum, chemical, food-processing...
Journal Articles
Alloy Digest (2011) 60 (3): Ni-688.
Published: 01 March 2011
... NAS 600 is a nickel alloy with 14-17 chromium and has excellent oxidation resistance. The alloy is used extensively in heat treatment furnaces. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes...
Journal Articles
Alloy Digest (2015) 64 (2): Ni-721.
Published: 01 February 2015
... DMV 600/600H are nickel alloys with 15.5 Cr. These stable, fully austenitic solid-solution alloys have higher carbon than alloy 600L (See Alloy Digest Ni-702, October 2012). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as...
Journal Articles
Alloy Digest (2020) 69 (4): Ni-758.
Published: 01 April 2020
... Special Metals Inconel Alloy 600 (UNS N06600 / Werkstoff Number 2.4816) is a nickel-chromium-iron alloy that is intended for corrosion-resistant and heat-resistant applications. Its versatility has led to its use in a variety of applications involving temperatures from cryogenic to above 1095 °C...
Journal Articles
Alloy Digest (1969) 18 (12): Ni-149.
Published: 01 December 1969
... Pyromet 600 is a corrosion-resisting nickel-base alloy, having a very desirable combination of high strength and workability, both hot and cold. It has high strength and resistance to oxidation at high temperatures. It is designed to meet the highest quality of the nuclear industry. This datasheet...
Journal Articles
Alloy Digest (1972) 21 (7): Ni-176.
Published: 01 July 1972
... INCONEL alloy 600 (formerly INCONEL, Alloy Digest Ni-9, March 1954) is a nickel-chromium-iron alloy with good resistance to corrosion and heat. It is a solid-solution alloy that can be hardened only by cold working and it has excellent mechanical properties with a desirable combination of high...
Journal Articles
Alloy Digest (1967) 16 (1): Ni-120.
Published: 01 January 1967
... RA-600 is a nickel-base chromium alloy having good oxidation resistance to 2150 F, and good resistance to carburizing and nitriding atmospheres. It is recommended for furnace construction and equipment. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1962) 11 (12): Ni-77.
Published: 01 December 1962
... RAonel 600 is a corrosion and heat resisting nickel-base alloy having a combination of high strength and oxidation resistance along with hot and cold workability. It is recommended for component parts in the aircraft, chemical, petroleum and paper pulp industries. This datasheet provides...
Journal Articles
Alloy Digest (1963) 12 (6): Ni-44.
Published: 01 June 1963
... UDIMET 600 is a vacuum-induction melted nickel-base alloy having excellent mechanical properties at high temperatures. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as forming, heat...
Journal Articles
Alloy Digest (1960) 9 (3): Ni-56.
Published: 01 March 1960
... INCONEL 600 nickel-base alloy has better high temperature properties than Inconel alloy, particularly where rupture strength, creep and short-time tensile are necessary. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as...
Journal Articles
Alloy Digest (2006) 55 (3): Ni-633.
Published: 01 March 2006
... Nicrimphy 600 is a nickel-base alloy designed to offer good corrosion and oxidation resistance. It also has good mechanical properties over a wide range of temperatures. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength. It...
Journal Articles
Alloy Digest (2021) 70 (1): SA-876.
Published: 01 January 2021
... Industeel Mars 600 is a medium-carbon, nickel-chromium-molybdenum-boron, alloy protection steel that is used in the quenched and tempered condition (typical hardness = 600 HBW). It is used not only as an add-on armor, but also as a structural material. This datasheet provides information on...
Journal Articles
Alloy Digest (2009) 58 (7): SA-604.
Published: 01 July 2009
... OvaX 600 is an ingot cast through-hardening steel that is specially designed for air hardening or gas quenching and for applications requiring isotropic properties and very high cleanliness levels. This datasheet provides information on composition, hardness, and tensile properties. It also...
Journal Articles
Alloy Digest (2009) 58 (10): SA-610.
Published: 01 October 2009
... steel ATI 600-MIL (Ultrahigh Hard Specialty Steel Armor) ATI 600-MIL Ultra High Hard is a specialty steel of wrought Ni-Cr-Mo steel for armor plate. ATI 600-MIL is trademark of ATI Properties, Inc. Patent application pending Chemical Composition, wt (Typical) Carbon 0.42 0.52 Nickel 3.75 4.25...
Journal Articles
Alloy Digest (2014) 63 (3): SA-696.
Published: 01 March 2014
... quenched. XAR 600 (Wear Resistant Structural Steel) XAR 600 Chemical Composition, wt (Maximum) Carbon 0.40 Silicon 0.80 Manganese 1.50 Phosphorus 0.025 Sulfur 0.010 Chromium 1.50 Molybdenum 0.50 Nickel 1.50 Boron 0.005 Iron bal The steel is produced with a fine-grained structure. The nitrogen is fixed as...
Journal Articles
Alloy Digest (2016) 65 (9): SA-765.
Published: 01 September 2016
... ABREX 600 (hardness target of 600 HBW) is one of the Abrex series of abrasion resistant steel plate alloys. Abrex 600 is a standard option. All of the products are maintained at very low impurity levels, making them well suited to welding and forming. This datasheet provides information on...
Journal Articles
Alloy Digest (2005) 54 (7): SA-548.
Published: 01 July 2005
... Chemical Composition, wt (Nominal) Carbon 0.15 Silicon 0.10 Manganese 1.3 Chromium 2.2 Nickel 0.5 Molybdenum 0.5 Vanadium 0.2 Iron bal Mechanical Properties: (Typical) Yield strength, 0.2%, min, MPa (ksi) Ovahyd 600 600 (87) Ovahyd 650 650 (94) Ovahyd 700 700 (102) Tensile strength, min, MPa (ksi) Ovahyd...
Journal Articles
Alloy Digest (1968) 17 (10): Ni-139.
Published: 01 October 1968
... NICKEL 201 is a low carbon version of Nickel 200 recommended for use in the electronic industries for service at temperatures between 600 F and 1200 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1981) 30 (9): Ni-270.
Published: 01 September 1981
... KANTHAL 70 alloy was designed to provide a high positive temperature coefficient to electrical resistance comparable with that of pure nickel; however, it has much higher electrical resistivity than pure nickel. This makes it useful as a voltage regulator when placed in series with another...
Journal Articles
Alloy Digest (1984) 33 (11): Ni-305.
Published: 01 November 1984
... INCO-WELD A Electrode is a nickel-base alloy developed for shielded metal-arc welding of INCONEL alloys 600 and 601 and INCOLOY alloy 800H to be exposed to elevated temperatures (up to about 1600 F). This electrode also is used widely for various dissimilar combinations of austenitic and ferritic...