1-20 of 382 Search Results for

NICKEL 220

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1978) 27 (2): Ni-254.
Published: 01 February 1978
... Nickel 220 is widely used as a base material for cathodes in electronic receiving tubes. Its composition is controlled closely because this is necessary for all alloys produced especially for use in cathodes. Nickel 220 is effective where fairly easy activation is required without liberating...
Journal Articles
Alloy Digest (2005) 54 (9): Cu-736.
Published: 01 September 2005
..., and sulfide/chloride environments, and high resistance to MARINEL® 220 Filing Code: Cu-736 Copper September 2005 MARINEL® 220 (Ultrahigh-Strength Copper-Nickel Alloy) Marinel 220 is a copper alloy of 18% Ni with high manganese and aluminum. It develops high strength with excellent corrosion resistance...
Journal Articles
Alloy Digest (1969) 18 (2): SS-220.
Published: 01 February 1969
... Croloy 18 13 3 is a chromium-nickel-molybdenum stainless steel characterized as having high corrosion resistance to certain acidic solutions. It is recommended for paper, chemical, and oil refining industries. This datasheet provides information on composition, physical properties, microstructure...
Journal Articles
Alloy Digest (1963) 12 (5): Ni-82.
Published: 01 May 1963
... CORRONEL 220 is a high molybdenum nickel-base alloy having high strength and high acid resistance. It is a vanadium stabilised variant of the alloy formerly known as CORRONEL B. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1975) 24 (8): Ni-220.
Published: 01 August 1975
.... Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys elasticity heat treatability heater elements joinability machinability physical properties TECHALLOY A tensile properties workability TECHALLOY A Filing Code: Ni-220 Nickel Alloy...
Journal Articles
Alloy Digest (2005) 54 (10): Cu-737.
Published: 01 October 2005
... to Marinel (see Alloy Digest Cu-602). It is a copper alloy with 18% nickel and high manganese and aluminum. It develops high strength with excellent corrosion resistance in seawa- ter. It is the successor alloy to Marinel 220 (see Alloy Digest Cu-736). Marinel is a registered trademark of Langley Alloys Ltd...
Journal Articles
Alloy Digest (1996) 45 (11): Fe-114.
Published: 01 November 1996
... Ni-Rod Filler Metal 44 is a solid, nickel-iron-manganese wire designed for automatic and semiautomatic welding of ductile, malleable, and gray cast irons in all positions. NI-Rod Filler Metal 44 offers high-speed, high-quality welds and can be used with all robotics, automatic, and semiautomatic...
Journal Articles
Alloy Digest (2001) 50 (3): Cu-660.
Published: 01 March 2001
... Wieland-K55 is a hardenable copper alloy with nickel and silicon. Mill hardened strip is used in connector applications. The alloy is produced under a license from Olin Brass, USA. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1953) 2 (5): Ni-4.
Published: 01 May 1953
... INCOLOY is a heat resistant iron alloy of high percentages of nickel and chromium. It provides a high temperature alloy with excellent resistance to oxidation, good strength at elevated temperatures, and good workability and welding properties. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2012) 61 (11): SA-667.
Published: 01 November 2012
... (particularly on Ni and Cr contents) and, possibly, on customer s specification. Carbon 0.22 Chromium 1.0 Nickel 2.0 Molybdenum 0.6 Manganese 1.50 Sulfur 0.005 Phosphorus 0.015 Silicon 0.5 Boron 0.005 Iron bal Physical Properties: Density, kg/m3 (lb/in.3) 8100 (0.29) Mechanical Properties: Tensile properties...
Journal Articles
Alloy Digest (2003) 52 (8): Cu-707.
Published: 01 August 2003
... Wieland-N17 has a combination of strength and favorable cold working and corrosion properties. Its composition gives it better protection to more severe atmospheres than other copper alloys. It is characterized by a high nickel content. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1972) 21 (1): SS-265.
Published: 01 January 1972
... CRUCIBLE 303 PLUS is an austenitic chromium-nickel stainless steel to which elements have been added to improve the machinability and non-galling characteristics. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (2020) 69 (9): TS-800.
Published: 01 September 2020
... CarTech L6 is an oil-hardening, high-carbon (0.70%), nickel-chromium, alloy cold-work tool steel. It is suitable for short run tooling in applications where a combination of high hardness and good toughness is required. The relatively high nickel content results in an alloy with greater impact...
Journal Articles
Alloy Digest (2021) 70 (4): Ni-769.
Published: 01 April 2021
... VDM 601 (Nicrofer 6023 H) is a nickel-chromium-iron alloy with additions of aluminum and titanium. This alloy is specifically recommended for service above 550 °C (1020 °F) because of its superior creep-rupture properties resulting from its controlled carbon content and coarse grain size...
Journal Articles
Alloy Digest (1987) 36 (11): Be-7.
Published: 01 November 1987
... nickel, chromium, gold, etc. Black anodizing produces a nonconductive coating that can be made reflective or matte. Chromate passivation extends shelf-life protection. Health Precautions: Care must be taken to avoid inhalation or airborne particulates in excess of 2 micrograms of beryllium per cubic...
Journal Articles
Alloy Digest (1992) 41 (10): Ni-413.
Published: 01 October 1992
... BRUSH WELLMAN Alloy 360 beryllium nickel strip combines unique mechanical and physical properties required in electrical, electronic and electromechanical systems. Strength, stress-relaxation and fatigue are some of those properties. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1962) 11 (3): Al-112.
Published: 01 March 1962
... aluminum alloys, as well as excel- lent machinability and corrosion resistance. The consequence of exceeding the impurity limits in the composition are such that high copper or nickel decreases resistance to corrosion, while high iron, silicon or manganese decreases me- chanical properties. If not properly...
Journal Articles
Alloy Digest (2018) 67 (8): Ni-746.
Published: 01 August 2018
... Composition, wt.% Carbon 0.10 max Manganese 0.10 0.30 Silicon 0.20 0.30 Phosphorus 0.020 max Sulfur 0.015 max Nickel 48.0 50.0 Chromium 48.0 50.0 Niobium 1.40 1.70 Iron 1.0 max Mechanical Properties See Table 1 and 2. Room temperature, minimum values, are shown below Tensile strength, MPa (ksi) 550 (79.8...
Journal Articles
Alloy Digest (1984) 33 (5): Fe-70.
Published: 01 May 1984
... MAGNIFER 50 is a soft magnetic iron-nickel alloy containing about 48% nickel. It has a saturation induction of 1.55T and a high permeability. It exhibits the highest saturation induction obtainable with iron-nickel alloys. Typical applications are (1) Low-frequency power transducers, (2) Chokes...
Journal Articles
Alloy Digest (1959) 8 (11): SA-92.
Published: 01 November 1959
... Silicon Nickel Chromium Molybdenum Iron 0.27 - 0.33 0.60 - 0.80 0.40 - 0.70 1.85 - 2.25 1.00 - 1.35 0.35 - 0.55 Remainder PROPERTIES Table 1 -HEAT TREATED TENSILE PROPERTIES+ (Oil quenched and tempered) Tempering Tensile Temperature Strength OF. psi Yield Strength psi (0.2% ) Elongation c~ in 2 Reduction...