1-20 of 33 Search Results for

NI-ROD FILLER METAL 99

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1996) 45 (4): Ni-507.
Published: 01 April 1996
... NI-Rod Filler Metal 99 is a commercially pure nickel solid wire developed for weld deposition on as-welded cast irons by automatic or semiautomatic processes. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on joining. Filing Code...
Journal Articles
Alloy Digest (2016) 65 (6): Ni-725.
Published: 01 June 2016
.... For welding, VDM Alloy 617 B should be in the solution annealed condition and be free from scale, grease, and markings. When welding roots, sufficient protection of the root needs to be ensured with pure argon (Ar 4.6) so that the welding seam is free of oxides. Fill Metal. The following filler materials...
Journal Articles
Alloy Digest (1963) 12 (2): Ni-79.
Published: 01 February 1963
... R-405 physical properties screw machines tensile properties workability MONEL ALLOY R-405 Filing Code: Ni-79 Nickel Alloy FEBRUARY 1963 -DATA ON WORLD WIDE METALS AND ALLOYS MONEL* Alloy R-405 (Machining Grade Nickel-Copper Alloy) niblisbed by Engineering Alloys Digest, Inc. Upper Montdair...
Journal Articles
Alloy Digest (2022) 71 (1): CS-214.
Published: 01 January 2022
... thickness, but not less than 1 h. Source: Ref 48 49 Table 25 Filler metal Welding process SMAW GMAW GTAW Filler metal AWS A5.1/A5.1M E7016(a) AWS A5.18/A5.18M ER70S-G(b)(c) AWS A5.18/A5.18M ER70S-G(d) (a) Equivalent Kobelco filler metal designation: Familiarc LB-52. The electrodes dried at the temperature...
Journal Articles
Alloy Digest (1974) 23 (7): SS-298.
Published: 01 July 1974
.... Joinability: Carpenter Stanless No. 7-Mo can be welded and brazed saris- factori& without any special precautions. Recommended weld- ing methods are tungsten inert-gas shielded-arc welding (TlG) with or without filler metal or metal arc welding with coated electrodes. Filler metal or rods of rhe ~-MO...
Journal Articles
Alloy Digest (2022) 71 (10): CS-233.
Published: 01 October 2022
... 1250) Peening may be necessary Yes (a) Soaking time = 1 h per 25 mm (1 in.) of maximum section thickness, but not less than 1 h. Source: Ref 50 51 Table 24 Filler metal Welding process SMAW GMAW GTAW Filler metal AWS A5.1/A5.1M E6013(a), AWS A5.1/A5.1M E6019(b), AWS A5.1/A5.1M E7016(c) AWS A5.18...
Journal Articles
Alloy Digest (2022) 71 (11): CS-234.
Published: 01 November 2022
... (a) Soaking time = 1 h per 25 mm (1 in.) of maximum section thickness, but not less than 1 h. Source: Ref 52 53 Table 24 Filler metal Welding process SMAW GMAW GTAW Filler metal AWS A5.1/A5.1M E6013(a), AWS A5.1/A5.1M E6019(b), AWS A5.1/A5.1M E7016(c) AWS A5.18/A5.18M ER70S-G(d)(e) AWS A5.18/A5.18M ER70S-G(f...
Journal Articles
Alloy Digest (2022) 71 (8): CS-229.
Published: 01 August 2022
... 4 Post weld heat treatment Desirable or optional Temperature range(a) °C (°F) Optional Optional 590 675 (1100 1250) Peening may be necessary Yes (a) Soaking time = 1 h per 25 mm (1 in.) of maximum section thickness, but not less than 1 h. Source: Ref 56, 58 Table 25 Filler metal Welding process...
Journal Articles
Alloy Digest (2022) 71 (8): CS-228.
Published: 01 August 2022
... Consumable. Table 26. Comparable Grades See Tables 27 29. Table 26 Filler metal Welding process SMAW GMAW GTAW Filler metal AWS A5.1/A5.1M E6013(a), AWS A5.1/A5.1M E6019(b), AWS A5.1/A5.1M E7016(c) AWS A5.18/A5.18M ER70S-G(d)(e) AWS A5.18/A5.18M ER70S-G(f) (a) Equivalent Kobelco filler metal designation...
Journal Articles
Alloy Digest (2022) 71 (5): CS-222.
Published: 01 May 2022
... section thickness, but not less than 1 h. Source: Ref 56 57 Table 26 Filler metal Welding process SMAW GMAW GTAW Filler metal AWS A5.1/A5.1M E6013(a), AWS A5.1/A5.1M E6019(b), AWS A5.1/A5.1M E7016(c) AWS A5.18/A5.18M ER70S-G(d)(e) AWS A5.18/A5.18M ER70S-G(f) (a) Equivalent Kobelco filler metal designation...
Journal Articles
Alloy Digest (2022) 71 (5): CS-223.
Published: 01 May 2022
... grain size of 7 (Ref 13). While calculating the ideal critical diameter it has been assumed that the limits for residual elements in both the SAE and EN ISO grades are identical, i.e., Cr 0.20 %, Mo 0.06 %, Ni 0.25 %, Cu 0.30 %. Alloy Digest: Data on Worldwide Metals and Alloys CS-223 / 3 Table...
Journal Articles
Alloy Digest (2022) 71 (6): CS-224.
Published: 01 June 2022
... 131 Alloy Digest: Data on Worldwide Metals and Alloys CS-224 / 3 Table 2 Mechanical properties at room temperature (continued) Diameter mm in. Thickness mm in. Rp0.2 MPa ksi MPa Rm ksi AZ %% KU J ft·lbf Hardness HBW Product form: bar, rod, forgings. Treatment condition: isothermal annealed...
Journal Articles
Alloy Digest (2022) 71 (11): CS-235.
Published: 01 November 2022
... Post weld heat treatment Desirable or optional Temperature range(a) °C (°F) Optional Optional 590 675 (1100 1250) Peening may be necessary Yes (a) Soaking time = 1 h per 25 mm (1 in.) of maximum section thickness, but not less than 1 h. Source: Ref 51 52 Table 23 Filler metal Welding process SMAW...
Journal Articles
Alloy Digest (2022) 71 (6): CS-225.
Published: 01 June 2022
... Thickness mm 50 > 50 100 in. 2 >2 4 Desirable or optional Optional Optional Temperature range(a) °C (°F) 590 675 (1100 1250) Peening may be necessary Yes (a) Soaking time = 1 h per 25 mm (1 in.) of maximum section thickness, but not less than 1 h. Source: Ref 61 62 Table 28 Filler metal Welding...
Journal Articles
Alloy Digest (1995) 44 (2): SS-583.
Published: 01 February 1995
...: For butt welding of tubes, the root pass is carried out with the TIC (GTAW) process with filler metal. The MMA process can be used for subsequent passes. In the case of welding tubes to tube sheeL the TIC process with filler metal is also necessary. The chemical composition of wire or rods must be selected...
Journal Articles
Alloy Digest (1982) 31 (5): Ni-275.
Published: 01 May 1982
.... To obtain elongations of more rhan 3Oqo after cold working in excess of 20070, the material must be heat treated. Welding: NICROFER 6020 HMO can be welded by conventional fusion welding processes, such as arc welding with coated electrodes, TIG or MIG with filler metals of the same alloy type. It can...
Journal Articles
Alloy Digest (2022) 71 (1): CS-215.
Published: 01 January 2022
... be necessary Yes Yes (a) Soaking time = 1 h per 25 mm (1 in.) of maximum section thickness, but not less than 1 h. Source: Ref 47 48 Table 28 Filler metal Welding process SMAW GMAW GTAW Filler metal AWS A5.5/A5.5M E9016-G(a) AWS A5.28/A5.28M ER90S-G(b) AWS A5.28/A5.28M ER80S-G(c) (a) Equivalent Kobelco...
Journal Articles
Alloy Digest (2022) 71 (7): CS-227.
Published: 01 July 2022
... elements in both the SAE and EN ISO grades are identical: Si = 0.15 0.30 %, Cr 0.20 %, Mo 0.06 %, Ni 0.25 %, Cu 0.30 % Alloy Digest: Data on Worldwide Metals and Alloys CS-227 / 3 Table 5 Compatibility of non-alloy steels with selected corrodents Environment(a) Acetaldehyde Acetic acid, all...
Journal Articles
Alloy Digest (2022) 71 (3): CS-218.
Published: 01 March 2022
... range(a) °C (°F) Desirable Desirable 590 675 (1100 1250) Desirable Peening may be necessary Yes Yes Yes (a) Soaking time = 1 h per 25 mm (1 in.) of maximum section thickness, but not less than 1 h. Source: Ref 51 52 Table 27 Filler metal Welding process SMAW GMAW GTAW Filler metal AWS A5.5/A5.5M E10016...
Journal Articles
Alloy Digest (2022) 71 (2): CS-217.
Published: 01 February 2022
... locations in the United States and Canada are given in Table 11. Source: Ref 26 27 Liquid-Metal Corrosion. Non-alloy steels can be embrittled by contact with liquid brass, aluminum bronze, copper, zinc, Table 2 Chemical composition of C45, C45E, and C45R Element C Si Mn P S Cr Mo Ni Cu Others Iron...