Alloy Digest (1993) 42 (8): SA-467.
Published: 01 August 1993
... NF616, nominally 9Cr-0.5 Mo-1.8W-Cb(Nb)-V, is an alloy in the 9 Cr system developed to overcome the disadvantages of high expansion with austenitic alloys for boiler operations, while maintaining high strength. NF 616 is expected to find use in boiler tubing and main steam piping. This datasheet...