1-4 of 4 Search Results for

NAS 660

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2014) 63 (11): SS-1189.
Published: 01 November 2014
... NAS 660 is a Ni-Cr stainless steel alloy with excellent heat resistance. The alloy is used for its high strength at high temperatures. The alloy is a precipitation-hardening material. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (2013) 62 (4): Ni-707.
Published: 01 April 2013
.... Specification Equivalents: UNS N06002 ASTM B435 JIS H4551 NW 6002 SAE AMS 5536 Table 1 Mechanical properties at room temperature 0.2% yield strength, MPa (ksi) Tensile strength, MPa (ksi) Elongation, % Hardness HV HR JIS H4551 / NW6002 245 ( 36) 660 ( 96) 35 ASTM B435 / UNS N6002 240 ( 35) 655...
Journal Articles
Alloy Digest (2002) 51 (12): Ni-595.
Published: 01 December 2002
... quenching or rapid air cooling is recommended, and it is essential to pre- vent precipitation. Stress equalizing by soaking for 1 2 h at 300 350 °C (570 660 °F) followed by air cooling is necessary with machined mate- rial to remove stress concentrations prior to age hardening. It may also be applied to...
Journal Articles
Alloy Digest (2004) 53 (11): SS-913.
Published: 01 November 2004
... 8.4 800 1472 1.40 842 25 14.4 630 0.150 135 19.6 53 7.7 1000 1832 1.45 872 28 16.2 660 0.158 120 17.4 48 7.0 Table 3 Typical Tensile Properties after Solution Annealing Heat Treatment Yield strength, Yield strength, Temperature 0.2% 1.0% Tensile strength Elongation, °C °F MPa ksi MPa ksi MPa ksi % 20...