1-20 of 24

Search Results for NAS 64

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2010) 59 (8): SS-1072.
Published: 01 August 2010
... NAS 64 is a duplex stainless steel with molybdenum for pitting and crevice corrosion resistance and a duplex microstructure for resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (2010) 59 (7): SS-1070.
Published: 01 July 2010
... Resistance: NAS 74N has excellent localized resistance against pitting crevice corrosion as well as superior acid resistance in comparison with general austenitic stainless steels such as AISI Types 304 and 316L, to NAS 329J3L (UNS S32205) and NAS 64. See also Table 3 and Fig. 1. Specification Equivalents...
Journal Articles
Alloy Digest (2013) 62 (3): SS-1140.
Published: 01 March 2013
... in comparison with SUS 304, SUS 316L, NAS 329J3L (UNS S32205), and NAS 64. See Fig. 1. Specification Equivalents: UNS S32760 ASTM A240 EN 1.4501 in EN 10088-2/10028-7 General Characteristics: A super duplex stainless steel with a pitting resistance equivalent (PRE) of at least 40, NAS 75N provides excellent...
Journal Articles
Alloy Digest (2017) 66 (6): SS-1267.
Published: 01 June 2017
... (3) 3273-4642 www.nyk.co.jp ISSN: 002-614X SS-1267B Table 1 Pitting corrosion resistance Alloy ASTM G48 Method A ASTM G48 Method C 22 °C (72 °F) 50 °C (122 °F) Critical pitting corrosion temperature CPT, °C (°F) NAS 255 × 50 (122) NAS 329J3L × 50 (122) NAS 64 55 (131) NAS 255NM 75 (167...
Journal Articles
Alloy Digest (2013) 62 (5): SS-1146.
Published: 01 May 2013
... (0.18) 71.91 (2.83) 764.93 (30.12) 704.46 (27.73) 33.74 (1.33) NAS 64 0.01 (0.0004) 0.02 (0.0008) 1.07 (0.04) 191.92 (7.56) 1053.96 (41.49) 60.72 (2.39) NAS 254N 0.02 (0.0008) 0.05 (0.002) 1.02 (0.04) 2.11 (0.08) 2.16 (0.09) 7.76 (0.31) NAS 155N 0.01 (0.0004) 0.02 (0.0008) 2.68 (0.11) 3.2 (0.13) 0.79...
Journal Articles
Alloy Digest (2010) 59 (3): SS-1059.
Published: 01 March 2010
... Material 30% (117 °C) 35% (126 °C) 42% (142 °C) NAS 155N O O X SUS 316L X X X NAS 64 X X X Test conditions: boiling MgCl 2 solution, 100 h. U-bending test. O, No cracks. X, cracks present Specification Equivalents: UNS S31727 ASTM A240 General Characteristics: NAS 155N (UNS S31727) is a stainless steel...
Journal Articles
Alloy Digest (2010) 59 (5): SS-1064.
Published: 01 May 2010
... NAS 64 38 (a) Atmospheric exposure test period of 2 years. (b) PRE (Pitting Resistance Evaluation) = %Cr + 3.3 X %Mo + 16 X %N : Without corrosion. With corrosion, maximum pit depth 15 m. With corrosion, maximum pit depth > 15 m ...
Journal Articles
Alloy Digest (2015) 64 (8): SS-1223.
Published: 01 August 2015
...) 35%, 126 °C (259°F) 30%, 115 °C (239 °F) 25%, 110 °C (230 °F) 20%, 108 °C (226 °F) Type 304 18Cr-8Ni X X X X X X X X Type 316L 17Cr-12Ni-2Mo X X X X X X X O NAS 329J3L 22Cr-5.3Ni-3.2Mo-0.16N X X X X X X O O NAS 64 25Cr-6Ni-3.3Mo-0.16N X X X X X X O O NAS 155N 18Cr-15Ni-4Mo-3Cu-0.15N X X X X X O O O...
Journal Articles
Alloy Digest (2020) 69 (6): Cu-909.
Published: 01 June 2020
... or source: Wieland Rolled Products NA. Producer or Source: Wieland Rolled Products NA Copyright © ASM International® 2020 2020 ASM International Wieland C21000 chemical composition physical properties elasticity high-temperature alloys workability heat treatability bullet jackets coined...
Journal Articles
Alloy Digest (2011) 60 (3): Ni-688.
Published: 01 March 2011
... treatment 732 (1350) 137 (20) 93 (14) 64 (9) 871 (1600) 56 (8) 36 (5) 25 (4) 982 (1800) 30 (4) 20 (3) 13 (2) Cold-rolled sheet, annealing 538 (1000) 511 (74) 345 (50) 234 (34) 649 (1200) 234 (34) 158 (23) 100 (15) 760 (1400) 89 (13) 58 (8) 38 (6) 871 (1600) 52 (8) 33 (5) 21 (3) Heat Treatment: NAS 600...
Journal Articles
Alloy Digest (2021) 70 (4): Cu-919.
Published: 01 April 2021
... Rolled Products NA. Producer or Source: Wieland Rolled Products NA Copyright © ASM International® 2021 2021 ASM International Wieland C22000 chemical composition physical properties tensile properties corrosion-resistant alloys workability heat treatability machinability UNS C22000...
Journal Articles
Alloy Digest (2017) 66 (1): Al-450.
Published: 01 January 2017
... (62) 6 5 77.9 (11.3) 79.3 (11.5) 2630 (0.095) 7075-T7351 (AMS 4078) 25.42 50.80 (1.001 2.000) 476 (69) 476 (69) 393 (57) 393 (57) na 6 71.0 (10.3) 73.0 (10.6) 2796 (0.101) 7050-T7451 (AMS 4050) 6.35 50.80 (1.001 2.000) 510 (74) 510 (74) 441 (64) 441 (64) 10 9 71.0 (10.3) 73.0 (10.6) 2823 (0.102) DOI...
Journal Articles
Alloy Digest (2017) 66 (3): Al-455.
Published: 01 March 2017
..., % Tension modulus, GPa (106 psi)L LT L LT L LT 2624-T351 (AMS 4464) 12.70 25.40 (0.500 1.000) 434 (63) 448 (65) 331 (48) 303 (44) 16 15 71.0 (10.3) 25.43 38.10 (1.001 1.500) 427 (62) 441 (64) 324 (47) 303 (44) 16 15 2024-T7351 (AMS 4037) 12.70 25.40 (0.500 1.000) 434 (63) 434 (63) 331 (48) 290 (42) NA 8...
Journal Articles
Alloy Digest (1959) 8 (3): TS-80.
Published: 01 March 1959
.... Quench it 67 6 2 50 2 39 38 1600°F. Quench 2 2: 3; 64 2i 44 DOI: 10.31399/asm.ad.ts0080 Copyright © ASM International® 1996 Table I-DEFORMATION RRSULTING FROM HARDENING+ Point of Testing Upper End Middle LOWEd Dimensions, Inches Before Hardening After Hardening 0. D. 2.748 2.7475 LD. 2.121 2.120 0. D...
Journal Articles
Alloy Digest (2004) 53 (11): SS-913.
Published: 01 November 2004
... are not recommended since intermetallic intergranular precipitations may occur at the fusion line. This alloy is less sensitive to hot cracking phenome- na than high-nickel heat-resistant steels. Neither prewelding nor SIRIUS S15 Filing Code: SS-913 Stainless Steel November 2004 SIRIUS S15 (Heat-Resistant Stainless...
Journal Articles
Alloy Digest (1962) 11 (2): TS-114.
Published: 01 February 1962
... indicated) As quenched 950 1000 1025 1050 1100 1150 1200 Rockwell Hardness CD, 64-65 67-69 67-69 67-69 67-69 65-67 63-65 59-61 B - (Auscenitized at 22OOoF in a salt bath, held one minute at hear, quenched in oil and tempered 2 t 2 t 2 hours at temperature indicated) Tempering Temperature Rockwell Hardness...
Journal Articles
Alloy Digest (1998) 47 (4): SS-711.
Published: 01 April 1998
... 123 34 54 4.88 0.192 25 794 115 945 137 35 69 4.70 0.185 30 918 133 1028 149 26 66 434 0.171 40 1035 150 1104 160 15 56 3.96 0.156 50 1173 170 1208 175 23 64 3.56 0.140 60 1214 176 1435 208 18 62 DOI: 10.31399/asm.ad.ss0711 Table 4 Typical Tensile Properties at Various Test Temperatures -73 -1cKl 490...
Journal Articles
Alloy Digest (1965) 14 (3): Cu-149.
Published: 01 March 1965
... 42000-55000 44000-59000 53000-66000 60000 -72000 68000-78000 78000-88000 Elongation % in 2 I 40-50 20-38 15-30 5-20 4-15 3-13 o-5 Rockwell Hardness B o-15 35-50 42-58 53-70 64-74 68-78 78-88 Table 3 - EFFECT OF ANNE.4LING COLD ROLLED hlATERI.4L Grain Tensile Rockwell Size Strength Elongation Hardness...
Journal Articles
Alloy Digest (1960) 9 (3): TS-91.
Published: 01 March 1960
... for tools requiring maximum wear. Pack in a box containing solid carburixing compound, heat to 1700-1750 F., hold at temperature for 3-4 hours, remove and quench in oil. (Na- turally the soaking time IS dependent upon the size of the tool and desired depth of case). TEMPERING: Temper immediately after...
Journal Articles
Alloy Digest (1995) 44 (11): Ni-491.
Published: 01 November 1995
... IodPF -200 0 20 100 200 300 400 500 600 700 800 900 loo0 -200 32 68 200 400 600 800 1000 1200 1400 1600 1800 150 0.045 78.5 426 0.102 71.5 456 0.109 70.5 475 0.113 66.5 500 0.132 61.5 570 0.139 57 530 0.124 56 525 0.128 57.5 535 0.130 60 550 62 565 0.133 64 580 0.137 66.5 590 0.144 69 540 500 490 465...