Publisher: Journals Gateway
Alloy Digest (2010) 59 (6): SS-1066.
Published: 01 June 2010
... NAS 354N is a super austenitic stainless steel with very high molybdenum for pitting and crevice corrosion resistance and high enough nickel content for good resistance to stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2015) 64 (9): SS-1225.
Published: 01 September 2015
... NAS 354N Type 316L 5 0.01 (0.0004) 0.01 (0.0004) 1.67 (0.07) 10 0.02 (0.0008) 0.03 (0.001) 4.69 (0.18) 20 0.03 (0.001) 0.03 (0.001) 71.97 (2.83) 40 0.03 (0.001) 2.06 (0.08) 764.93 (30.12) 60 0.03 (0.001) 3.02 (0.12) 704.46 (27.74) 80 3.27 (0.13) 4.98 (0.20) 33.74 (1.33) Results of immersion test...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2010) 59 (7): SS-1070.
Published: 01 July 2010
... acid is used in pickling. To the extent the NAS 354N is more resistant to corrosion than AISI Type 304, descaling is more difficult. Alkaline immersion for a short time before acid pickling and shot blasting, if possible, are effective at descaling. Workability: Care should be taken when cold working...