Alloy Digest (2011) 60 (5): SS-1092.
Published: 01 May 2011
... NAS 329J3L is a duplex stainless steel with molybdenum for pitting and crevice corrosion resistance and for resistance to stress-corrosion cracking, a duplex microstructure. The title covers two alloys, the latter with restricted chemistry, inside the other. This datasheet provides information...
Journal Articles
Alloy Digest (2010) 59 (7): SS-1070.
Published: 01 July 2010
... Resistance: NAS 74N has excellent localized resistance against pitting crevice corrosion as well as superior acid resistance in comparison with general austenitic stainless steels such as AISI Types 304 and 316L, to NAS 329J3L (UNS S32205) and NAS 64. See also Table 3 and Fig. 1. Specification Equivalents...
Journal Articles
Alloy Digest (2012) 61 (3): Ni-696.
Published: 01 March 2012
...) > 120 (> 248) NAS NW276 > 120 (> 248) > 120 (> 248) NAS 254N 80 (176) 80 (176) NAS 329J3L 50 (122) 45 (113) SUS 316L 10 (50) 25 (77) Table 3 Crevice corrosion resistance Alloy Critical pitting corrosion temperature (CCT), ºC (ºF) 6% FeCl3 + 1% HCl solution (ASTM G48 Method D) Green death solution NAS...
Journal Articles
Alloy Digest (2017) 66 (6): SS-1267.
Published: 01 June 2017
... (3) 3273-4642 www.nyk.co.jp ISSN: 002-614X SS-1267B Table 1 Pitting corrosion resistance Alloy ASTM G48 Method A ASTM G48 Method C 22 °C (72 °F) 50 °C (122 °F) Critical pitting corrosion temperature CPT, °C (°F) NAS 255 × 50 (122) NAS 329J3L × 50 (122) NAS 64 55 (131) NAS 255NM 75 (167...
Journal Articles
Alloy Digest (2010) 59 (11): Ni-681.
Published: 01 November 2010
... 2 Corrosion resistance Pitting corrosion resistance Alloy Critical pitting corrosion temperature [CPT], ºC (ºF) 6% FeCl 3 + 1% HCl solution, (ASTM G48 Method C) Green death solution NAS NW276 > 120 (> 248) > 120 (> 248) NAS 254N 80 (176) 80 (176) NAS 329J3L 50 (122) 45 (113) SUS 316L 10 (50) 25 (77...
Journal Articles
Alloy Digest (2013) 62 (3): SS-1140.
Published: 01 March 2013
... in comparison with SUS 304, SUS 316L, NAS 329J3L (UNS S32205), and NAS 64. See Fig. 1. Specification Equivalents: UNS S32760 ASTM A240 EN 1.4501 in EN 10088-2/10028-7 General Characteristics: A super duplex stainless steel with a pitting resistance equivalent (PRE) of at least 40, NAS 75N provides excellent...
Journal Articles
Alloy Digest (2012) 61 (2): Ni-694.
Published: 01 February 2012
... Corrosion resistance to sulfuric acid Fig. 2 Pitting and crevice corrosion resistance Table 2 Stress corrosion cracking resistance Solution (a) SUS 316L NAS 329J3L NAS 825 NAS 254N Boiling 42% MgCl 2 × × × × Boiling 35% MgCl 2 × × Boiling 25% MgCl 2 × Boiling 20% MgCl 2 Stress corrosion...
Journal Articles
Alloy Digest (2015) 64 (8): SS-1223.
Published: 01 August 2015
...) 35%, 126 °C (259°F) 30%, 115 °C (239 °F) 25%, 110 °C (230 °F) 20%, 108 °C (226 °F) Type 304 18Cr-8Ni X X X X X X X X Type 316L 17Cr-12Ni-2Mo X X X X X X X O NAS 329J3L 22Cr-5.3Ni-3.2Mo-0.16N X X X X X X O O NAS 64 25Cr-6Ni-3.3Mo-0.16N X X X X X X O O NAS 155N 18Cr-15Ni-4Mo-3Cu-0.15N X X X X X O O O...