Alloy Digest (2010) 59 (5): SS-1064.
Published: 01 May 2010
... NAS 254N is a high performance corrosion resistance austenitic stainless steel with resistance to hot sea water. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as...
Journal Articles
Alloy Digest (2010) 59 (11): Ni-681.
Published: 01 November 2010
... 2 Corrosion resistance Pitting corrosion resistance Alloy Critical pitting corrosion temperature [CPT], ºC (ºF) 6% FeCl 3 + 1% HCl solution, (ASTM G48 Method C) Green death solution NAS NW276 > 120 (> 248) > 120 (> 248) NAS 254N 80 (176) 80 (176) NAS 329J3L 50 (122) 45 (113) SUS 316L 10 (50) 25 (77...
Journal Articles
Alloy Digest (2012) 61 (3): Ni-696.
Published: 01 March 2012
... solution NAS NW22 > 120 (> 248) > 120 (> 248) NAS NW276 > 120 (> 248) > 120 (> 248) NAS 254N 80 (176) 80 (176) NAS 329J3L 50 (122) 45 (113) SUS 316L 10 (50) 25 (77) Table 3 Crevice corrosion resistance Alloy Critical pitting corrosion temperature (CCT), ºC (ºF) 6% FeCl3 + 1% HCl solution (ASTM G48 Method D...
Journal Articles
Alloy Digest (2013) 62 (5): SS-1146.
Published: 01 May 2013
...) Type 316L 1.67 (0.07) 4.69 (0.18) 71.91 (2.83) 764.93 (30.12) 704.46 (27.73) 33.74 (1.33) NAS 64 0.01 (0.0004) 0.02 (0.0008) 1.07 (0.04) 191.92 (7.56) 1053.96 (41.49) 60.72 (2.39) NAS 254N 0.02 (0.0008) 0.05 (0.002) 1.02 (0.04) 2.11 (0.08) 2.16 (0.09) 7.76 (0.31) NAS 155N 0.01 (0.0004) 0.02 (0.0008...
Journal Articles
Alloy Digest (2012) 61 (2): Ni-694.
Published: 01 February 2012
... Corrosion resistance to sulfuric acid Fig. 2 Pitting and crevice corrosion resistance Table 2 Stress corrosion cracking resistance Solution (a) SUS 316L NAS 329J3L NAS 825 NAS 254N Boiling 42% MgCl 2 × × × × Boiling 35% MgCl 2 × × Boiling 25% MgCl 2 × Boiling 20% MgCl 2 Stress corrosion...