Alloy Digest (1994) 43 (12): SA-481.
Published: 01 December 1994
... NAK 55 is a very clean steel for use in plastic and rubber molds were impact resistance is not critical in design. Its age-hardening gives very high strength and good wear resistance. Tight tolerance are obtained with consistent expansion and contraction properties. This datasheet provides...
Journal Articles
Alloy Digest (1995) 44 (8): Co-98.
Published: 01 August 1995
... to a great extent on many different parts, including: shaft sleeves, various pump components, bushings. buffing fixtures, cutting tool chip breakers and high tempera- ture (900┬░F) unlubricated sleeve bearings operating in liquid sodium, liquid potassium, and NaK. Applications: Wal1ex-cobah-base alloys have...