Alloy Digest (2021) 70 (9): Cu-924.
Published: 01 September 2021
... Mueller Brass C38500 is a wrought copper-zinc-lead alloy (leaded brass) that is suitable for high-speed screw machining applications and moderate thread rolling. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...