Alloy Digest (1962) 11 (3): Cu-115.
Published: 01 March 1962
... Mueller 799 tellurium copper combines the high electrical and thermal conductivity and corrosion resistance of copper with the excellent machinability of free turning brass. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1980) 29 (2): Cu-389.
Published: 01 February 1980
... MUELLER Alloy 1450 (formerly MBCo Alloy 799) is a high-conductivity copper containing sufficient small copper telluride particles to provide free-machining characteristics superior to those of any other high-conductivity copper. It has the same general corrosion resistance as copper. It is used...