Alloy Digest (1969) 18 (1): Cu-195.
Published: 01 January 1969
... Mueller 6730 is a forgeable (leaded) bronze bearing alloy possesing good machinability for use with hard or soft mating members where moderate strength will suffice. It is recommended for gears, pump parts, thrust bearings, valve seats, etc. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1984) 33 (11): Cu-486.
Published: 01 November 1984
... Company. Producer or Source: Mueller Brass Company Copyright ┬ę ASM International┬« 1996 1996 ASM International bearings bushings chemical composition connecting rods corrosion-resistant alloys elasticity hardness heat treatability joinability machinability MUELLER ALLOY 6730...