Alloy Digest (1970) 19 (3): Cu-212.
Published: 01 March 1970
... MUELLER 6162 is a general purpose alloy for use where high strength and corrosion resistance are necessary, but where high hardness is not a factor. It is recommended for fasteners, bearings, valve stems, gears and pole line hardware. This datasheet provides information on composition, physical...