Alloy Digest (1991) 40 (12): Ni-398.
Published: 01 December 1991
... MUMETAL is a very high permeability soft magnetic alloy. (See also Alloy Digest Ni-25, April 1956.) This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating. Filing Code: Ni-398. Producer or source...
Journal Articles
Alloy Digest (1956) 5 (4): Ni-25.
Published: 01 April 1956
... MUMETAL is a high permeability nickel iron alloy to be used where high permeability at flux densities well under 5000 gausses is desirable. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (1969) 18 (4): Ni-144.
Published: 01 April 1969
... drawn shields, consideration should be given to the use of the more ductile alloy, such as Mumetal). The use of protective atmosphere, preferably commercial hydrogen, will obviate the necessity for removing scale which might be detrimental to subsequent drawing operations. It is to be noted...