1-2 of 2 Search Results for

Monel alloy 401

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1970) 19 (6): Cu-216.
Published: 01 June 1970
... MONEL alloy 401 is a copper-nickel alloy with high electrical resistance and is used primarily in specialized electrical and electronic applications. It has a negligible temperature coefficient of electrical resistance and good corrosion resistance. This datasheet provides information...
Journal Articles
Alloy Digest (2000) 49 (3): TS-574.
Published: 01 March 2000
... Co. Monel and Inconel are registered trademarks of Special Metals Corpora- tion. Chemical Composition, wt (Nominal) Carbon 0.55 Manganese 0.80 Nickel 1.55 Chromium 0.90 Molybdenum 0.30 Copper 0.75 Iron Balance Heat Treatment: In all cases soak at temperature for 1 h per inch of least dimen- sion...