Alloy Digest (1969) 18 (4): Ni-144.
Published: 01 April 1969
... Allegheny Ludlum Moly Permalloy is a nickel-iron-molybdenum alloy having excellent permeability and core loss properties. It has high initial and maximum permeability, low coercive force, and low hysteresis loss. It is recommended for toroids, tape and lamination cores. This datasheet provides...
Journal Articles
Alloy Digest (2001) 50 (1): Fe-4.
Published: 01 January 2001
... field levels in combination with Moly Permalloy. Also the material can be used in high-frequency transformer applications and, in the past, has been used in telecommunication applications. AL 4750 alloy is sold in two grades rotor, which is a fine-grained, equalized structure with a cube on face texture...