Alloy Digest (1956) 5 (4): Mg-24.
Published: 01 April 1956
... MELTRON AZ855 is a magnesium forging alloy recommended for large forgings requiring high tensile strength, fatigue endurance and ductility, combined with good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...