Alloy Digest (2021) 70 (2): CI-78.
Published: 01 February 2021
... Meehanite GC275 is a pearlitic gray cast iron that has a minimum tensile strength of 275 MPa (40 ksi) when determined on test pieces machined from separately cast, 30 mm (1.2 in.) diameter, test bars. This intermediate-tensile-strength grade has a fine, close-grained structure that is ideal for...