Alloy Digest (1954) 3 (9): CI-8.
Published: 01 September 1954
... MEEHANITE GC is a high strength iron casting having high damping capacity, self-lubricating properties, and good machinability. It combines the good properties of both cast iron and steel. Applications include machine tools, gears, shafts, housings, permanent molds, lathe beds, bases, pistons...