Skip Nav Destination
Close Modal
Search Results for
Meehanite AQ
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2 Search Results for
Meehanite AQ
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1970) 19 (10): CI-36.
Published: 01 October 1970
... MEEHANITE AQ is a wear and abrasion resisting iron that is readily machinable as cast but may be air hardened after machining with minimum distortion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear...
Abstract
View article
PDF
MEEHANITE AQ is a wear and abrasion resisting iron that is readily machinable as cast but may be air hardened after machining with minimum distortion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on high temperature performance as well as heat treating and machining. Filing Code: CI-36. Producer or source: Meehanite Metal Corporation.
Journal Articles
Alloy Digest (1964) 13 (5): CI-33.
Published: 01 May 1964
... designations as AQS-HS and WS. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on casting, heat treating, machining, and joining. Filing Code: CI-33. Producer...
Abstract
View article
PDF
DUCTLIRON is a high-carbon ferrous material containing graphite in the form of nodules or spheroids. It possesses unusually high ductility, strength and castability. It is furnished in three different grades, namely, SF-60, SP-80 and SH-100. Alloyed grades are also available under different designations as AQS-HS and WS. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on casting, heat treating, machining, and joining. Filing Code: CI-33. Producer or source: Rosedale Foundry.