Alloy Digest (1969) 18 (9): SA-243.
Published: 01 September 1969
... McLOUTH ML-F is a fine grained high-strength low-alloy steel suited for difficult stamped and drawn parts. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive, shear, and bend strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (1966) 15 (5): SA-194.
Published: 01 May 1966
... McLouth ML-50 is a high-strength low-alloy steel combining excellent formability, weldability with good atmospheric corrosion resistance. It is recommended for structural components where decreased weight is desired. This datasheet provides information on composition, physical properties, hardness...