Alloy Digest (1996) 45 (1): SS-633.
Published: 01 January 1996
... Crucible Maxel 2000 is a corrosion resistant, pre-hardened, free machining steel based on AISI 414 (Alloy Digest SS-103, February 1989) stainless steel. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1996) 45 (2): SS-637.
Published: 01 February 1996
... alloy steel holder block or P-20 steel, and it is comparable to 420 mold steel in similar heat-treated condi- tions. It will resist attacks from cooling water, condensation, humidity and some mild acids. For more severe environments. the higher corrosion resistance of MAXEL 2000 (Alloy Digm SS-633) may...
Journal Articles
Alloy Digest (2003) 52 (11): SS-894.
Published: 01 November 2003
... environment such as stronger acids or higher concentrations of chlorides or bromides may in fact cause corrosion in SCM 420XL. As shown below, both CMS 21XL (see Alloy Digest SS620) and Maxel 2000 (see Alloy Digest SS-633) are more corrosion resistant than CSM 420XL and may be better suited for use...