Skip Nav Destination
Close Modal
Search Results for
Manaurite XMR
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Subjects
Journal
Article Type
Date
Availability
1-2 of 2 Search Results for
Manaurite XMR
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2019) 68 (1): Ni-749.
Published: 01 January 2019
... Manaurite XMR is a heat resistant alloy for hydrocarbon processing. It is a modified version of Manaurite XM (Alloy Digest Ni-748, December 2018) designed to withstand creep elongation at high temperature, while also being able to be welded after aging. This datasheet provides information...
Abstract
View article
PDF
Manaurite XMR is a heat resistant alloy for hydrocarbon processing. It is a modified version of Manaurite XM (Alloy Digest Ni-748, December 2018) designed to withstand creep elongation at high temperature, while also being able to be welded after aging. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on joining. Filing Code: Ni-749. Producer or source: Manoir Pîtres.
Journal Articles
Alloy Digest (2018) 67 (12): ni-748.
Published: 01 December 2018
... radiant coils for cracking furnaces and for high severity furnaces. Fig. 1 Comparative 100, 000 hours creep rupture data Manaurite XMR vs Manaurite XM Producer Manoir Pitres 27108 Val de Reuil, Cedex, France Tel: +33 2 324 87200 Fax: + 33 2 324 95726 www.manoir-industries.com ISSN: 002-604X DOI: 10.31399...
Abstract
View article
PDF
Manaurite XM is a heat resistant alloy for hydrocarbon processing. It is a microalloyed evolution of Manaurite 36X (Alloy Digest SS-1296, May 2018). This datasheet provides information on composition and physical properties as well as creep. It also includes information on joining. Filing Code: Ni-748. Producer or source: Manoir Pîtres.