Skip Nav Destination
Close Modal
Search Results for
Magnolia B-1
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1
Search Results for Magnolia B-1
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1997) 46 (1): Cu-609.
Published: 01 January 1997
... Magnolia B-1 is a lead-free copper alloy. It machines easier than the leaded SAE 660 alloy that it was designed to duplicate. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Abstract
View articletitled, <span class="search-highlight">MAGNOLIA</span> <span class="search-highlight">B</span>-<span class="search-highlight">1</span>: Lead-Free Machinable Bronze Casting Alloy
View
PDF
for article titled, <span class="search-highlight">MAGNOLIA</span> <span class="search-highlight">B</span>-<span class="search-highlight">1</span>: Lead-Free Machinable Bronze Casting Alloy
Magnolia B-1 is a lead-free copper alloy. It machines easier than the leaded SAE 660 alloy that it was designed to duplicate. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on casting, machining, and joining. Filing Code: CU-609. Producer or source: I. Schumann Company.