Alloy Digest (1996) 45 (7): Ni-514.
Published: 01 July 1996
... Technologies Corporation. Producer or Source: VDM Technologies Corporation Copyright ┬ę ASM International┬« 1996 1996 ASM International chemical composition Magnifier 53 physical properties thermal properties - DIGE! 9 I WA A A~IIw-FA@ PA 1 Filing Code: Ni-514 m Nickel Alloy ah r I- 0 -- 5...
Journal Articles
Alloy Digest (1996) 45 (8): Fe-111.
Published: 01 August 1996
... Magnifier 36 is a soft-magnetic nickel-iron alloy with 36% nickel. It has a saturation induction of 1.3 T and a rather high electrical resistance of 0.75 0.75 ohm mm 2 /m. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes...