Alloy Digest (1957) 6 (10): Mg-34.
Published: 01 October 1957
... MAGNESIUM ZK51A is a zirconium type magnesium sand casting alloy recommended for applications requiring high yield strength and uniformity of properties. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength...
Journal Articles
Alloy Digest (1959) 8 (6): Mg-5.
Published: 01 June 1959
...: I:IL8213 ASTM B-80, Alloy ZK51A Manufacturer: Magnesium Elektron Ltd., Manchester, England Licensees: Howard Foundry Company, Chicago, Illinois Rolle Manufacturing Co., Inc., Lansdale, Pennsylvania Aluminum Laboratories Limited, Montreal. Canada The Robert Mitchell Co. Limited, Montreal, Canada ...