Journal Articles
Alloy Digest (1963) 12 (1): Mg-54.
Published: 01 January 1963
... Magnesium QE-22A is a heat treatable magnesium-silver-zirconium rare earth casting alloy having very high yield strength at temperatures up to 500 F. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well...