Alloy Digest (1958) 7 (7): Mg-39.
Published: 01 July 1958
... Magnesium HK31 is a magnesium-base alloy possessing extraordinary resistance to creep and maintaining excellent strength through the temperature range of 300-700 F. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive, shear...