Journal Articles
Publisher: Journals Gateway
Alloy Digest (1958) 7 (6): Mg-38.
Published: 01 June 1958
... MAGNESIUM AZ92A is a good structural magnesium alloy particularly suitable for castings of variable wall thickness. It responds o an age-hardening heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1966) 15 (7): Mg-61.
Published: 01 July 1966
...: Magnesium die castings are not conside, ed weldable. Broken castings may be welded in the field to effect a temporary repair by gas welding with oxyacetylene or oxycarbo- hydrogen along with Dow flux No. 460 and magnesium AZ92A rod. Parts are preheated to about 7000F. The edges should be thoroughly cleaned...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1969) 18 (10): Mg-67.
Published: 01 October 1969
... shielded-arc in helium or argon is recommended. Oxyacetylene torch welding with fluxed elec- trode can also be used, but magnesium is susceptible to corrosive action of the welding flux used and care must be taken to remove the flux immediately after welding. Magnesium AZ92A, AZIOIA and ZK61A welding...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1954) 3 (10): Mg-13.
Published: 01 October 1954
... for tished parts. Specification Equivalents: ASTM B93-AZ92A; B80-AZ92A; B199-AZ92A Alcoa 260 Army 57-74-1 and 57-74-2 SAP 500 and 503 AMS 4434 and 4484 Federal QQ-M-55 and QQ-M-56 Alloy AZ92 MIL-R-6944 General Characteristics: Dowmeral C is a heat treatable casting type magnesium alloy. It is used for both...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1966) 15 (6): Mg-60.
Published: 01 June 1966
... Magnesium ZK21A is a non-hardenable extruded magnesium-base alloy having moderate strength and good weldability. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive strength. It also includes information on forming, heat treating...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1960) 9 (8): Mg-47.
Published: 01 August 1960
... temperature 1350-1550┬░F Add aluminum as aluminum or Al-Mn alloy; add zinc as zinc; add manganese as 95Al-5Mn. Use magnesium melting flux. Weldability: Readily welded by the inert-gas-shielded arc method. using filler metal of same composition or alloy AZ92A. Corrosion Resistance: Resistance to corrosion...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (10): Mg-78.
Published: 01 October 2011
... ELEKTRON AZ31B is a wrought magnesium alloy developed to offer good properties maintaining corrosion resistance and weldability. The alloy is used in aerospace, automotive, and military applications. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1957) 6 (2): Mg-31.
Published: 01 February 1957
... DOW AZ81A is a heat treatable magnesium alloy containing aluminum and zinc as its primary alloying elements. It is exclusively a sand-casting alloy. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive, shear...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1959) 8 (8): Mg-43.
Published: 01 August 1959
... and then boiling 2 hours in 5% sodium dichromate solution. Use Dow 450 welding flux for oxyacetylene gas weld- ing. Magnesium alloy 6ller rod is used in welding and should be AZ&A or AZ92A composition. Corrosion Resistance: Magnesium AZ6lA does not corrode in dry air, but develops a thin gray oxide ti in moist air...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1961) 10 (2): Mg-49.
Published: 01 February 1961
... welding flux for oxyacetylene gas welding. Magnesium alloy filler rod is used in welding and should be AZ92A composition. Specification Equivalents: ASTM B93-57T (Ingot) ASTM BSO-57T (Sand Castings) ASTM Bl99-57T (Permanent Mold Castings) Federal QQ-M-55 Alloy Al0 (Permanent Mold Castings) SAE 502...