Alloy Digest (1985) 34 (4): Cu-495.
Published: 01 April 1985
... MUELLER Copper 1220 is a deoxidized copper with high residual phosphorus (nominally 0.02%). It has rather low electrical conductivity but it is not susceptible to embrittlement by hydrogen. Its low electrical conductivity is mainly caused by the phosphorus. It has excellent cold-working...