Skip Nav Destination
Close Modal
Search Results for
MUELLER ALLOY 6731
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2
Search Results for MUELLER ALLOY 6731
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1984) 33 (6): Cu-478.
Published: 01 June 1984
... MUELLER Alloy 6731 is a free-cutting heat-treatable bearing bronze for use where no cold working of the metal is required. It is supplied only as forgings for use against hard mating members. It has excellent mechanical and wear properties for bearings and gears. It can be soldered readily. Its...
Abstract
View articletitled, <span class="search-highlight">MUELLER</span> <span class="search-highlight">ALLOY</span> <span class="search-highlight">6731</span>: Forgeable Leaded Bearing <span class="search-highlight">Alloy</span>
View
PDF
for article titled, <span class="search-highlight">MUELLER</span> <span class="search-highlight">ALLOY</span> <span class="search-highlight">6731</span>: Forgeable Leaded Bearing <span class="search-highlight">Alloy</span>
MUELLER Alloy 6731 is a free-cutting heat-treatable bearing bronze for use where no cold working of the metal is required. It is supplied only as forgings for use against hard mating members. It has excellent mechanical and wear properties for bearings and gears. It can be soldered readily. Its applications include pump barrels, bearings, gears and bushings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-478. Producer or source: Mueller Brass Company.
Journal Articles
Alloy Digest (1967) 16 (9): Cu-180.
Published: 01 September 1967
... Dynalloy 6731 (formerly Mueller alloy 603) is a forgeable bearing bronze having excellent mechanical and wear properties for gears and bearings, combined with good machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Abstract
View articletitled, DYNALLOY <span class="search-highlight">6731</span>(603): Bronze Gear <span class="search-highlight">Alloy</span>
View
PDF
for article titled, DYNALLOY <span class="search-highlight">6731</span>(603): Bronze Gear <span class="search-highlight">Alloy</span>
Dynalloy 6731 (formerly Mueller alloy 603) is a forgeable bearing bronze having excellent mechanical and wear properties for gears and bearings, combined with good machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-180. Producer or source: Mueller Brass Company.