Alloy Digest (1979) 28 (2): Cu-366.
Published: 01 February 1979
... MUELLER Alloy 4640 (formerly MBCo Alloy 203) is a classic marine alloy known as Naval Brass. It contains nominally 0.75% tin which has made it the most widely used marine alloy. It is suitable for both salt and fresh water applications. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1978) 27 (10): Cu-361.
Published: 01 October 1978
... MUELLER Alloy No. 6300 (formerly MBCo. Alloy 224K and sometimes called Tuf-Stuf Alloy) is a heat-treatable aluminum bronze containing 5% nickel. It is intended for those applications requiring combinations of corrosion resistance, excellent bearing properties at considerable loads, and extremely...
Journal Articles
Alloy Digest (1954) 3 (4): Cu-15.
Published: 01 April 1954
..., propeller hub cones, drill jigs, molds, rollers, lead screw nuts and clutch shifter forks. Manufacturer: Mueller Brass Company Port Huron, Michigan 1Or DIGEST CARPENTER No. 5-876 Rltgc kfA-8 -w DECRMEER 19E2 DATA ON WORLD WIDE METALS AND ALLOYS Publisbcd by Eogineaing Alloys Digesf Inc upper W New J-w...