Alloy Digest (1980) 29 (10): Cu-404.
Published: 01 October 1980
... MUELLER Alloy 3771 (formerly MBCo. Alloy 211) is one of the most widely used and most easily forged of the copper-base forging alloys. It is most often used in multiple sequence hammer forging operations where a wide forging temperature range is desired. It is also a free-machining alloy. Typical...