Skip Nav Destination
Close Modal
Search Results for
MUELLER ALLOY 3602
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
MUELLER ALLOY 3602
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1985) 34 (1): Cu-489.
Published: 01 January 1985
... MUELLER Alloy 3602 is a leaded brass of moderate strength and ductility. It is suitable for moderate thread rolling. Also, because of its free-cutting characteristics, it is suitable for high-speed screw-machine products. Among its many applications are hardware, unions, bolts, screws and nuts...
Abstract
View article
PDF
MUELLER Alloy 3602 is a leaded brass of moderate strength and ductility. It is suitable for moderate thread rolling. Also, because of its free-cutting characteristics, it is suitable for high-speed screw-machine products. Among its many applications are hardware, unions, bolts, screws and nuts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-489. Producer or source: Mueller Brass Company.