Alloy Digest (1981) 30 (11): Cu-425.
Published: 01 November 1981
... MUELLER Alloy 3300 is a brass containing 0.5% lead for improving machinability. The lead detracts somewhat from its cold workability; however, despite the lead, cold workability is rated as excellent. Overall, the alloy has a good to excellent combination of machinability and cold workability...