Alloy Digest (1972) 21 (11): Cu-262.
Published: 01 November 1972
... MUELLER ALLOY No. 1470 is a high-conductivity copper containing sulfur to promote free-machining properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (1982) 31 (7): Cu-440.
Published: 01 July 1982
... ON WORLD WIDE METALS AND ALLOYS @ Copyright 1980, Engineering Publications, Inc. AtI rights reserved. ISSN:OOZ-614X Pubhhed by Xg&wZg=& hJ- Upper Montchir, New Jersey MUELLER COPPER 1470 (Sulfur-Bearing High-Conductivity Copper) MUELLER COPPER 1470 is a high-conductivity copper to which sulfur has been...
Journal Articles
Alloy Digest (2013) 62 (5): Cu-818.
Published: 01 May 2013
... Mueller Alloy C36500 has excellent machining characteristics. The alloy is often called Leaded Muntz Metal, uninhibited. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating...