Alloy Digest (2017) 66 (9): SA-798.
Published: 01 September 2017
... MTD 3 is a Mn-Cr-Mo-V plate steel used in cavity molds. ArcelorMittal USA MTD steels comprise a family of prehardened alloy plate steels developed for a variety of mold, tool, and die applications. This datasheet provides information on composition. It also includes information on forming, heat...
Journal Articles
Alloy Digest (1997) 46 (1): SA-484.
Published: 01 January 1997
.... All the Lukens steels are produced in a modem elect& melt shop, which includes a 165 ton electric arc fumace. a ladle furnace for steel relining, and a tank degasser for vacuum treamxn~ When specified for MTD 3 (only). a very clean steel with sulfur levels as low as 0.001% maximum can be produced...
Journal Articles
Alloy Digest (2017) 66 (10): SA-801.
Published: 01 October 2017
... steel is water quenched and tempered to 262 321 HB to 76 mm (3 in.) inclusive and 241 321 over 76 165 mm (3 6.5 in inclusive. Machining: These steels are usually machined by grinding, milling, and drilling. Thermal Cutting: As with any steel having high carbon and alloy levels, MTD steels, if thermally...
Journal Articles
Alloy Digest (2017) 66 (11): SA-804.
Published: 01 November 2017
...) gascut hot, mm (in.) Preheat 149 ºC (300 ºF) gascut hot immediately heat treat edges, mm (in.) MTD 1 25.4 (1.0) and under Over 25.4 (1) MTD 2 25.4 (1.0) and under Over 25.4 (1) MTD 3 All thicknesses MTD 4 All thicknesses MTD P20 All thicknesses DOI: 10.31399/asm.ad.sa0804 Two additional heat...
Journal Articles
Alloy Digest (2017) 66 (7): SA-793.
Published: 01 July 2017
... applications. Chemical Composition, wt Carbon 0.38 0.46 Sulfur 0.040 max Phosphorus 0.035 max Silicon 0.15 0.40 Manganese 0.70 1.00 Chromium 0.80 1.15 Molybdenum 0.15 0.25 Vanadium 0.03 min Iron bal Heat Treatments: MTD 1 steel is normalized and tempered to 262 321 HB in thicknesses to 73 mm (3 in.) and 241...
Journal Articles
Alloy Digest (2017) 66 (8): SA-794.
Published: 01 August 2017
... for thermal cutting ArcelorMittal USA specifications Preheat 149 ºC (300 ºF) gascut hot Preheat 149 ºC (300 ºF) gascut hot immediately heat treat edges MTD 1 25.4 mm (1.0 in.) and under Over 25.4 mm (1 in.) MTD 2 25.4 mm (1.0 in.) and under Over 25.4 mm (1 in.) MTD 3 All thicknesses MTD 4 All thicknesses...
Journal Articles
Alloy Digest (1967) 16 (9): SS-200.
Published: 01 September 1967
..., aircraft mtd missile structural compcments. jet a+ cmpa~~ents. MOtWfOCtU~r: Practically all alloy md sraialcss steel mills. ...