Alloy Digest (2017) 66 (8): SA-794.
Published: 01 August 2017
... MTD 2 is mold base quality, Mn-Cr-Mo plate steel. It is commonly used in holder blocks, clamping plates, and support plates. ArcelorMittal USA MTD steels comprise a family of pre-hardened alloy plate steels developed for a variety of mold, tool, and die applications. This datasheet provides...
Journal Articles
Alloy Digest (2017) 66 (9): SA-798.
Published: 01 September 2017
... furnaces, all with the latest process control features. MTD is a registered trademark of Arcelor Mittal USA. Table 1 Recommended practice for thermal cutting ArcelorMittal USA specifications Preheat 149 ºC (300 ºF) gascut hot Preheat 149 ºC (300 ºF)(a) MTD 1 25.4 mm ( 1.0 in.) >25.4 mm (>1 in.) MTD 2...
Journal Articles
Alloy Digest (2017) 66 (11): SA-804.
Published: 01 November 2017
...) gascut hot, mm (in.) Preheat 149 ºC (300 ºF) gascut hot immediately heat treat edges, mm (in.) MTD 1 25.4 (1.0) and under Over 25.4 (1) MTD 2 25.4 (1.0) and under Over 25.4 (1) MTD 3 All thicknesses MTD 4 All thicknesses MTD P20 All thicknesses DOI: 10.31399/asm.ad.sa0804 Two additional heat...
Journal Articles
Alloy Digest (2017) 66 (10): SA-801.
Published: 01 October 2017
... (300 ºF), gascut hot immediately heat treat edges MTD 1 25.4 mm ( 1.0 in.) >25.4 mm (>1 in.) MTD 2 25.4 mm ( 1.0 in.) >25.4 mm (>1 in.) MTD 3 All thicknesses MTD 4 All thicknesses MTD P20 All thicknesses DOI: 10.31399/asm.ad.sa0801 MTD plates are prehardened and tempered in one of three...
Journal Articles
Alloy Digest (2017) 66 (7): SA-793.
Published: 01 July 2017
... is a registered trademark of Arcelor Mittal USA. Table 1 Recommended practice for thermal cutting ArcelorMittal USA specifications Preheat 149 ºC (300 ºF) gascut hot Preheat 149 ºC (300 ºF) gascut hot immediately heat treat edges MTD 1 25.4 mm (1.0 in.) and under Over 25.4 mm (1 in.) MTD 2 25.4 mm (1.0...
Journal Articles
Alloy Digest (1997) 46 (1): SA-484.
Published: 01 January 1997
... of applications including holder blocks. Lukens MTD 1 steel is normal&d and tempemd to 262 to 32 1 HB in thicknesses to 3 in. and 241 to 321 HB over 3 in. to 6l/2 in. Lukens MTD 2 is a mold base quality M&r-MO plate steel. It is commonly used in holder blocks. clamping plates, and support plates. The typical 0.29...
Journal Articles
Alloy Digest (1967) 16 (9): SS-200.
Published: 01 September 1967
..., aircraft mtd missile structural compcments. jet a+ cmpa~~ents. MOtWfOCtU~r: Practically all alloy md sraialcss steel mills. ...