1-7 of 7 Search Results for

MTD 1

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2017) 66 (7): SA-793.
Published: 01 July 2017
... MTD 1 is a 4140 plate steel modified with slightly higher carbon and a vanadium addition. Vanadium improves graining refinement and, coupled with the higher carbon, promotes hardness and wear resistance. ArcelorMittal USA MTD steels comprise a family of pre-hardened alloy plate steels developed...
Journal Articles
Alloy Digest (1997) 46 (1): SA-484.
Published: 01 January 1997
.... Thermal Cutting: As with any steel having high carbon and alloy levels, MTD steels, if thermally cut should be preheated and then stress relieved as detailed in Table 1. More details on this processing are available from the producer. Table 1 Thermal Cutting Heat Treat Practice T . ,ip Fldws~, hkat300-F...
Journal Articles
Alloy Digest (2017) 66 (9): SA-798.
Published: 01 September 2017
...: As with any steel having high carbon and alloy levels, MTD steels, if thermally cut, should be preheated and then stress relieved as detailed in Table 1. More details are available from the producer. Copyright © 2017, ASM International®. All rights reserved. MTD® 3 (Prehardened Engineering Steel) Filing Code...
Journal Articles
Alloy Digest (2017) 66 (11): SA-804.
Published: 01 November 2017
... and tempered in one of three continuous heat-treating facilities or in car bottom heat treating furnaces, all with the latest process control features. MTD is a registered trademark of Arcelor Mittal USA. Table 1 Recommended practice for thermal cutting ArcelorMittal USA specifications Preheat 149 ºC (300 ºF...
Journal Articles
Alloy Digest (2017) 66 (10): SA-801.
Published: 01 October 2017
... gage control to produce plates with uniform thickness end-to-end and side-to-side with mill-edge quality available. MTD is a registered trademark of ArcelorMittal USA. Table 1 Recommended practice for thermal cutting ArcelorMittal USA specifications Preheat 149 ºC (300 ºF) gascut hot Preheat 149 ºC...
Journal Articles
Alloy Digest (2017) 66 (8): SA-794.
Published: 01 August 2017
... processing. Thermal Cutting: As with any steel having high carbon and alloy levels, MTD steels, if thermally cut, should be preheated and then stress relieved as detailed in Table 1. Recommended practices are based on Tables 10 and 11, Iron and Steel Society Steel Products Manual-Plates, and/or ArcelorMittal...
Journal Articles
Alloy Digest (1967) 16 (9): SS-200.
Published: 01 September 1967
..., aircraft mtd missile structural compcments. jet a+ cmpa~~ents. MOtWfOCtU~r: Practically all alloy md sraialcss steel mills. ...