Journal Articles
Alloy Digest (1957) 6 (2): Ti-11.
Published: 01 February 1957
... MST Grae III is commercially pure, unalloyed titanium made by the Method S melting process, offering improved weldability and impact strength This datasheet provides information on composition, physical properties, hardness, tensile properties, and bend strength as well as fracture toughness...