1-1 of 1 Search Results for

MST 881

Sort by
Journal Articles
Alloy Digest (1960) 9 (5): Ti-25.
Published: 01 May 1960
... MST 881 is a titanium alloy capable of holding properties to 1100 F. It extends the useful temperature range of titanium alloys to 1100 F for long-time applications and to 1600 F for short-time applications. This datasheet provides information on composition, physical properties, elasticity...