Alloy Digest (1965) 14 (3): Ti-4.
Published: 01 March 1965
... MST 3AL-5CR is a double melted titanium base alloy available in either ingot, bar, rod, plate, forging, or extrusion form. It possesses good creep and high strength properties at room and elevated temperatures to 800 deg. F. This datasheet provides information on composition, physical properties...