Alloy Digest (1998) 47 (11): SS-733.
Published: 01 November 1998
... MO-RE 10MA is a fully austenitic heat-resistant casting alloy with microalloy additions. This alloy has exceptional strength and superior carburization resistance for extended service. Typical uses include pyrolysis and reformer tubing. This datasheet provides information on composition, physical...