Alloy Digest (2006) 55 (9): SA-556.
Published: 01 September 2006
... Mittal Di-Form T500 is a dual-phase steel intended primarily for exposed outer automotive body panels (door, hoods, and fenders). Dual-phase steels are one of the important advanced high-strength steel products developed for the automotive industry. Their microstructure typically consists...