Alloy Digest (1984) 33 (6): Ni-298.
Published: 01 June 1984
... METGLAS MBF-90/MBF-90A is a brazing foil in ductile, flexible metallic-glass form (a similar grade, MBF-90, is identical except that is has larger dimensional tolerances. It is suitable for joining stainless steels and superalloys, including those containing aluminum and titanium. It provides high...
Journal Articles
Alloy Digest (1984) 33 (4): Ni-296.
Published: 01 April 1984
... METGLAS MBF-35A is a brazing foil in ductile flexible metallic-glass form (a similar grade, MBF-35, is identical except that it has larger dimensional tolerances. It is a low-temperature filler metal foil designed for joining superalloys where the brazing operation should be done simultaneously...