Alloy Digest (1981) 30 (11): Ni-272.
Published: 01 November 1981
... METGLAS MBF-10A is a brazing foil in ductile, flexible metallic-glass form (a similar grade, MBF-10, is identical except that it has larger dimensional tolerances). This foil provides an alloy with high strength at both elevated and room temperatures. It can be used to join highly stressed...