1-1 of 1 Search Results for

MAXIVAL MVAPM

Sort by
Journal Articles
Alloy Digest (2006) 55 (6): SS-966.
Published: 01 June 2006
... Maxival MVAPM is an enhanced-machining version of AISI Type 316 stainless steel. The alloy has a specified inclusion picture to enhance machining by modifying both sulfide and oxide inclusions. This datasheet provides information on composition, hardness, and tensile properties. It also includes...