Skip Nav Destination
Close Modal
Search Results for
MAXITE
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
MAXITE
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1986) 35 (7): TS-461.
Published: 01 July 1986
... MAXITE is a tungsten-cobalt-vanadium high-speed tool steel. It is best used when maximum chip removal with single-point cutting tools is of primary importance. Tools made from Maxite will cut tough and hard materials such as stainless steels and hardened alloy steels with relative ease...
Abstract
View article
PDF
MAXITE is a tungsten-cobalt-vanadium high-speed tool steel. It is best used when maximum chip removal with single-point cutting tools is of primary importance. Tools made from Maxite will cut tough and hard materials such as stainless steels and hardened alloy steels with relative ease. It is excellent for cutting weld flashings and gritty, scaly hard castings. Among its many applications are drills, lathe tools, planer tools, cutoff tools and roll-turning tools. This datasheet provides information on composition and hardness. It also includes information on wear resistance as well as forming, heat treating, and machining. Filing Code: TS-461. Producer or source: Columbia Tool Steel Company.