Alloy Digest (1996) 45 (2): SS-637.
Published: 01 February 1996
... Maxel 400 FM is a corrosion resistant pre-hardened, free machining steel intended for use as a holder or backing in plastic molding. Maxel 400 FM is similar to conventional 420 mold steel, but sulfur has been added to enhance its machining properties. This datasheet provides information...